Great thanks for the replies. Know what to do if there is a next time (

)
Did the original Thursday arvo' last week thinking - getting set for the W/E. Since I tried to rev' up the reaction with some heat Sunday arvo' + sunny spot today, the mix on the board has 70 - 80 % cured so there are a few patches of tacky but it is hardening - phew - did not relish the clean off.
I went with the polyester resin as there are a number places the foam core is visible and do not want to 'melt' it with epoxy. Plan to do some "Q"-cell filler jobs and sand out before the glass work. - Will get fresh ingredients - did not know catalyst could go off - this stuff would be 2 1/2 years old by now.
With epoxy I rely on 25 + minutes (in 24-28 deg' C) before any warming in the mix - but the mix ratios are much easier to judge.
Polyester catalyst at 1% mix (used an old kids panadol syringe) is fiddly and still not sure how long I have got - not much point mixing more than 100 mls if it goes off quickly.
Is there a guide to controlling the cure time?
CMC - polyester filler?? - sounds great - I have some car bog but it is a bit heavy - I normally use 'Q' cell mix in epoxy resin and planned to do the same with polyester resin.
Could try some of that water proof epoxy putty - looks like a swiss roll - slice some off and knead till the outer skin (my stuff has a green colour) = hardner blends in then mould on / shape - and sand once hardens - apparently can use when wet. Not sure about melting the core of a surf board though (a bit too xxy 4 this project).
Cheers