Ramona said..
I have posted about a comparison test I carried out a few years ago but it's probably time to repeat. I gathered a few sea shells together and set up glass jars with different cleaners to compare with Metal Gleam. I have used Metal Gleam since the mid 1980's to clean fibreglass and remove rust etc so I knew it worked. All the other professional fishermen used it and dairy farmers and shipwrights used it. My younger son was also the quality control chemist at the factory where it was made for several years. For the comparison I used the metal gleam at 5:1. CLR I think I used at their strongest recommendation . Vinegar was at full strength and I think at 50%. I put the same amount of shells in each jar and started the timing. The metal gleam immediately foamed up and completely dissolved the shells in 15 minutes or so. The CLR and vinegar mixtures had a few bubbles form but that was it.I left them for a few days but they did nothing. I also had a cast iron engine block I put some Metal gleam mixture in. I placed some brass and bronze bits into it and left overnight. They ended up shiny but undamaged. After another week or so they looked the same.
From the Metal Gleam safety data sheet:
3. COMPOSITION INFORMATION
Phosphoric acid 30 - 60 % (w/w)
Ingredients determined to be Non-Hazardous Balance
____________
100%
For general cleaning of stainless steel and my boat hull and deck I use 85% phosphoric acid (sourced online, link provided above) diluted one part to two or three water plus a good squirt of detergent as a surfactant to help the solution stick to surfaces. Then I rinse off after a couple minutes. I don't doubt that metal gleam might do a better job not knowing what other additives they have in there, but I am guessing to descale a heat exchanger it is the acid that is doing the job.
I accidentally splashed some of my mixture on my freshly painted cockpit when cleaning some old bolts and nuts and didn't wash it off and it bleached and damaged the brand new 2 pack polyurethane.